Negative annealing in silicon after the implantation of high-energy sodium ions


Cite item

Full Text

Open Access Open Access
Restricted Access Access granted
Restricted Access Subscription Access

Abstract

The implantation of sodium ions with an energy of 300 keV is carried out into high-resistivity p-Si. The annealing of defects at Tann = 350–450°C and related activation of atoms (the latter occurs at the “tail” of atom distribution) are described by a first-order reaction. At Tann = 450–525°C and irrespective of the ion dose, negative annealing is observed; this annealing is accompanied by an appreciable increase in the surface resistance ρs. According to estimations, the activation energy of this process amounts to ~2 eV. It is our opinion that the annealing is related to the precipitation of sodium donor atoms, which occurs at a depth exceeding by two–three times the projected range Rp of ions. The annealing of defects at Tann = 525–700°C, which leads to a further decrease in ρs, features an activation energy of ~2.1 eV. The hypothesis that the “tail” in the profiles of sodium atoms measured by secondary-ion mass spectroscopy is due to the diffusion of these atoms from the walls of the crater to its center is verified. It is shown that this process is not implemented since the profiles of sodium atoms measured at room temperature do not differ from those measured at–140°C.

About the authors

V. M. Korol’

Institute of Physics

Author for correspondence.
Email: vkorol@ctsnet.ru
Russian Federation, Rostov-on Don, 344090

A. V. Zastavnoi

Institute of Physics

Email: vkorol@ctsnet.ru
Russian Federation, Rostov-on Don, 344090

Yu. Kudriavtsev

Department Ingenieria Electrica–SEES

Email: vkorol@ctsnet.ru
Mexico, Mexico, 07360

R. Asomoza

Department Ingenieria Electrica–SEES

Email: vkorol@ctsnet.ru
Mexico, Mexico, 07360


Copyright (c) 2017 Pleiades Publishing, Ltd.

This website uses cookies

You consent to our cookies if you continue to use our website.

About Cookies