Thermoelectric properties of Bi2Te2.4Se0.6 solid solutions of different particle-size composition


Citar

Texto integral

Acesso aberto Acesso aberto
Acesso é fechado Acesso está concedido
Acesso é fechado Somente assinantes

Resumo

The thermoelectric properties of n-type Bi2Te2.4Se0.6 solid solution prepared by the vacuum hot pressing of powder mixtures with different particle sizes are investigated. The powders were prepared by the mechanical grinding of ingots and melt spinning. The microstructure and fracture pattern of a sample cleavage surface are analyzed using scanning electron microscopy and optical microscopy. The thermoelectric characteristics (the Seebeck coefficient, electrical conductivity, and thermal conductivity) are measured at room temperature and in the temperature range of 100–700 K.

Sobre autores

L. Ivanova

Baikov Institute of Metallurgy and Materials Science

Autor responsável pela correspondência
Email: ivanova@imet.ac.ru
Rússia, Moscow, 119334

Yu. Granatkina

Baikov Institute of Metallurgy and Materials Science

Email: ivanova@imet.ac.ru
Rússia, Moscow, 119334

L. Petrova

Baikov Institute of Metallurgy and Materials Science

Email: ivanova@imet.ac.ru
Rússia, Moscow, 119334

I. Nikhezina

Baikov Institute of Metallurgy and Materials Science

Email: ivanova@imet.ac.ru
Rússia, Moscow, 119334

A. Malchev

Baikov Institute of Metallurgy and Materials Science

Email: ivanova@imet.ac.ru
Rússia, Moscow, 119334

V. Alenkov

Scientific-Production Association “Crystal”

Email: ivanova@imet.ac.ru
Rússia, Korolev, 141060

S. Kichik

Scientific-Production Association “Crystal”

Email: ivanova@imet.ac.ru
Rússia, Korolev, 141060

A. Melnikov

Scientific-Production Association “Crystal”

Email: ivanova@imet.ac.ru
Rússia, Korolev, 141060


Declaração de direitos autorais © Pleiades Publishing, Ltd., 2017

Este site utiliza cookies

Ao continuar usando nosso site, você concorda com o procedimento de cookies que mantêm o site funcionando normalmente.

Informação sobre cookies