Preparation and catalase activity of gold-ceria composites
- 作者: Eryomin A.1, Abakshonok A.1, Agabekov V.1, Kvasyuk A.1
-
隶属关系:
- Institute of New Materials Chemistry
- 期: 卷 87, 编号 10 (2017)
- 页面: 2358-2368
- 栏目: Article
- URL: https://journals.rcsi.science/1070-3632/article/view/221426
- DOI: https://doi.org/10.1134/S1070363217100176
- ID: 221426
如何引用文章
详细
Gold-ceria composites (СеО2)Au and (Au)CeO2 which exhibited catalase activity towards H2O2 decomposition in an aqueous medium depending on their preparation conditions were formed in two stages in situ. In the presence of hydrazine dihydrochloride both the probability of the ceria formation and the catalase activity of (СеО2)Au were found to decrease. The catalase activity was at a maximum for (СеО2)Au when the gold nanoparticles were formed in the 1.0 mM HAuCl4 medium and for (Au)CeO2 when they were synthesized in 0.5–0.75 mM HAuCl4 and 1.0 mM Na3C6H5O7. Boiling (СеО2)Au and (Au)CeO2 composites at ~80 kPa reduced their capacity to decompose H2O2.
作者简介
A. Eryomin
Institute of New Materials Chemistry
编辑信件的主要联系方式.
Email: yan47@mail.ru
白俄罗斯, ul. F. Skoriny 36, Minsk, 2200141
A. Abakshonok
Institute of New Materials Chemistry
Email: yan47@mail.ru
白俄罗斯, ul. F. Skoriny 36, Minsk, 2200141
V. Agabekov
Institute of New Materials Chemistry
Email: yan47@mail.ru
白俄罗斯, ul. F. Skoriny 36, Minsk, 2200141
A. Kvasyuk
Institute of New Materials Chemistry
Email: yan47@mail.ru
白俄罗斯, ul. F. Skoriny 36, Minsk, 2200141