Gold-ceria composites (СеО2)Au and (Au)CeO2 which exhibited catalase activity towards H2O2 decomposition in an aqueous medium depending on their preparation conditions were formed in two stages in situ. In the presence of hydrazine dihydrochloride both the probability of the ceria formation and the catalase activity of (СеО2)Au were found to decrease. The catalase activity was at a maximum for (СеО2)Au when the gold nanoparticles were formed in the 1.0 mM HAuCl4 medium and for (Au)CeO2 when they were synthesized in 0.5–0.75 mM HAuCl4 and 1.0 mM Na3C6H5O7. Boiling (СеО2)Au and (Au)CeO2 composites at ~80 kPa reduced their capacity to decompose H2O2.

Об авторах

A. Eryomin

Institute of New Materials Chemistry

Автор, ответственный за переписку.
Email: yan47@mail.ru
Белоруссия, ul. F. Skoriny 36, Minsk, 2200141

A. Abakshonok

Institute of New Materials Chemistry

Email: yan47@mail.ru
Белоруссия, ul. F. Skoriny 36, Minsk, 2200141

V. Agabekov

Institute of New Materials Chemistry

Email: yan47@mail.ru
Белоруссия, ul. F. Skoriny 36, Minsk, 2200141

A. Kvasyuk

Institute of New Materials Chemistry

Email: yan47@mail.ru
Белоруссия, ul. F. Skoriny 36, Minsk, 2200141

Дополнительные файлы

Доп. файлы
Действие
1. JATS XML

© Pleiades Publishing, Ltd., 2017

Согласие на обработку персональных данных

 

Используя сайт https://journals.rcsi.science, я (далее – «Пользователь» или «Субъект персональных данных») даю согласие на обработку персональных данных на этом сайте (текст Согласия) и на обработку персональных данных с помощью сервиса «Яндекс.Метрика» (текст Согласия).