Cavitation-Erosion Wear Resistance of Fluoroplasticics in Model Food Production Media
- Авторлар: Stechishin M.S.1, Martynyuk A.V.1, Oleksandrenko V.P.1, Bilyk Y.M.1
-
Мекемелер:
- Khmelnitskii National University
- Шығарылым: Том 40, № 5 (2019)
- Беттер: 468-474
- Бөлім: Article
- URL: https://journals.rcsi.science/1068-3666/article/view/229348
- DOI: https://doi.org/10.3103/S1068366619050179
- ID: 229348
Дәйексөз келтіру
Аннотация
The effect of acidic, alkaline and neutral media on wear kinetics and mechanism for fluoroplastics and polyolefins has been studied. Equations for fluoroplastic and polyolefin wear intensity are obtained based on the thermochemical and mechanical model of their destruction. The values of the activation energies for the surface destruction onset over the entire wear cycle of the polymer surface spherulite are determined.
Негізгі сөздер
Авторлар туралы
M. Stechishin
Khmelnitskii National University
Хат алмасуға жауапты Автор.
Email: m-mezon@ukr.net
Украина, Khmelnitskii, 29016
A. Martynyuk
Khmelnitskii National University
Email: m-mezon@ukr.net
Украина, Khmelnitskii, 29016
V. Oleksandrenko
Khmelnitskii National University
Email: m-mezon@ukr.net
Украина, Khmelnitskii, 29016
Yu. Bilyk
Khmelnitskii National University
Email: m-mezon@ukr.net
Украина, Khmelnitskii, 29016
Қосымша файлдар