Wear resistance of electrospark WC–Cо coatings with different iron contents
- Autores: Burkov A.A.1
-
Afiliações:
- Institute of Materials of Far Eastern Branch of the Russian Academy of Sciences
- Edição: Volume 37, Nº 4 (2016)
- Páginas: 385-388
- Seção: Article
- URL: https://journals.rcsi.science/1068-3666/article/view/228424
- DOI: https://doi.org/10.3103/S1068366616040048
- ID: 228424
Citar
Resumo
The work presents the results of investigating the influence of the ion concentration in the WC‒Co electrode materials on the structure and properties of the coatings deposited by electrospark deposition (ESD) on low-carbon steel. It has also been shown that iron concentration affects the character of mass transfer and thickness of the deposited coating. The phase composition, roughness, and wear resistance of the obtained coatings were studied under the conditions of the dry microabrasive rubbing. The increased iron concentration in the electrode materials was found to intensify the decarbidization of tungsten carbide at ESA.
Palavras-chave
Sobre autores
A. Burkov
Institute of Materials of Far Eastern Branch of the Russian Academy of Sciences
Autor responsável pela correspondência
Email: burkovalex@mail.ru
Rússia, ul. Tikhookeanskaya 153, Khabarovsk, 680042
Arquivos suplementares