The wear of direct and reverse friction pairs made of TiC–ZhS6U titanium carbide-based metal–ceramic material and the metal component of this material, i.e., the ZhS6U nickel-base casting superalloy, has been studied. Both uncoated friction pairs and pairs with TiN and TiC coatings have been tested under a load of 2 N at a velocity of sliding of 0.15 m/s. It has been found that TiC–ZhS6U + TiC–TiC–ZhS6U + TiC has the highest wear resistance.

作者简介

L. Shuster

Ufa State Aviation Technical University

Email: chertovskikh@mail.ru
俄罗斯联邦, ul. K. Marksa 12, Ufa, 450000

R. Mamleyev

OOO MAROMA Technologies

Email: chertovskikh@mail.ru
俄罗斯联邦, pr. Oktyabrya 69/2, Ufa, 450054

R. Kamaletdinova

Ufa State Aviation Technical University

Email: chertovskikh@mail.ru
俄罗斯联邦, ul. K. Marksa 12, Ufa, 450000

S. Chertovskikh

Ufa State Aviation Technical University

编辑信件的主要联系方式.
Email: chertovskikh@mail.ru
俄罗斯联邦, ul. K. Marksa 12, Ufa, 450000

R. Kireev

Ufa State Aviation Technical University

Email: chertovskikh@mail.ru
俄罗斯联邦, ul. K. Marksa 12, Ufa, 450000

补充文件

附件文件
动作
1. JATS XML

版权所有 © Allerton Press, Inc., 2016