Effects of Decreasing the Initial Rolling Temperature in Three-High Roughing Stands


如何引用文章

全文:

开放存取 开放存取
受限制的访问 ##reader.subscriptionAccessGranted##
受限制的访问 订阅存取

详细

Research on expanding the product range and minimizing the energy costs at a linear medium-bar mill with three-high roughing stands is discussed. The possibility of controlling the mechanical properties of the product by decreasing the initial rolling temperature is considered. Despite the improvement in mechanical properties, decrease in the initial rolling temperature in the range 900–950°C is accompanied by increase in current load at the primary drive and decrease in dimensional precision of the product.

作者简介

E. Smirnov

Stary Oskol Technical Institute

编辑信件的主要联系方式.
Email: stalevoz@i.ua
俄罗斯联邦, Stary Oskol, 309516

A. Smirnov

Physicotechnical Institute of Metals and Alloys

Email: stalevoz@i.ua
乌克兰, Kiev, 03142

V. Sklyar

Stary Oskol Technical Institute

Email: stalevoz@i.ua
俄罗斯联邦, Stary Oskol, 309516

V. Belevitin

South Ural State Humanitarian and Pedagogical University

Email: stalevoz@i.ua
俄罗斯联邦, Chelyabinsk, 454080

S. Eron’ko

Donetsk National Technical University

Email: stalevoz@i.ua
乌克兰, Donetsk, 83001

R. Pivovarov

Stary Oskol Technical Institute

Email: stalevoz@i.ua
俄罗斯联邦, Stary Oskol, 309516

补充文件

附件文件
动作
1. JATS XML

版权所有 © Allerton Press, Inc., 2018