Effects of Decreasing the Initial Rolling Temperature in Three-High Roughing Stands
- Авторлар: Smirnov E.N.1, Smirnov A.N.2, Sklyar V.A.1, Belevitin V.A.3, Eron’ko S.P.4, Pivovarov R.E.1
-
Мекемелер:
- Stary Oskol Technical Institute
- Physicotechnical Institute of Metals and Alloys
- South Ural State Humanitarian and Pedagogical University
- Donetsk National Technical University
- Шығарылым: Том 48, № 6 (2018)
- Беттер: 381-387
- Бөлім: Article
- URL: https://journals.rcsi.science/0967-0912/article/view/180171
- DOI: https://doi.org/10.3103/S0967091218060104
- ID: 180171
Дәйексөз келтіру
Аннотация
Research on expanding the product range and minimizing the energy costs at a linear medium-bar mill with three-high roughing stands is discussed. The possibility of controlling the mechanical properties of the product by decreasing the initial rolling temperature is considered. Despite the improvement in mechanical properties, decrease in the initial rolling temperature in the range 900–950°C is accompanied by increase in current load at the primary drive and decrease in dimensional precision of the product.
Авторлар туралы
E. Smirnov
Stary Oskol Technical Institute
Хат алмасуға жауапты Автор.
Email: stalevoz@i.ua
Ресей, Stary Oskol, 309516
A. Smirnov
Physicotechnical Institute of Metals and Alloys
Email: stalevoz@i.ua
Украина, Kiev, 03142
V. Sklyar
Stary Oskol Technical Institute
Email: stalevoz@i.ua
Ресей, Stary Oskol, 309516
V. Belevitin
South Ural State Humanitarian and Pedagogical University
Email: stalevoz@i.ua
Ресей, Chelyabinsk, 454080
S. Eron’ko
Donetsk National Technical University
Email: stalevoz@i.ua
Украина, Donetsk, 83001
R. Pivovarov
Stary Oskol Technical Institute
Email: stalevoz@i.ua
Ресей, Stary Oskol, 309516
Қосымша файлдар