Effects of Decreasing the Initial Rolling Temperature in Three-High Roughing Stands


Цитировать

Полный текст

Открытый доступ Открытый доступ
Доступ закрыт Доступ предоставлен
Доступ закрыт Только для подписчиков

Аннотация

Research on expanding the product range and minimizing the energy costs at a linear medium-bar mill with three-high roughing stands is discussed. The possibility of controlling the mechanical properties of the product by decreasing the initial rolling temperature is considered. Despite the improvement in mechanical properties, decrease in the initial rolling temperature in the range 900–950°C is accompanied by increase in current load at the primary drive and decrease in dimensional precision of the product.

Об авторах

E. Smirnov

Stary Oskol Technical Institute

Автор, ответственный за переписку.
Email: stalevoz@i.ua
Россия, Stary Oskol, 309516

A. Smirnov

Physicotechnical Institute of Metals and Alloys

Email: stalevoz@i.ua
Украина, Kiev, 03142

V. Sklyar

Stary Oskol Technical Institute

Email: stalevoz@i.ua
Россия, Stary Oskol, 309516

V. Belevitin

South Ural State Humanitarian and Pedagogical University

Email: stalevoz@i.ua
Россия, Chelyabinsk, 454080

S. Eron’ko

Donetsk National Technical University

Email: stalevoz@i.ua
Украина, Donetsk, 83001

R. Pivovarov

Stary Oskol Technical Institute

Email: stalevoz@i.ua
Россия, Stary Oskol, 309516

Дополнительные файлы

Доп. файлы
Действие
1. JATS XML

© Allerton Press, Inc., 2018

Согласие на обработку персональных данных

 

Используя сайт https://journals.rcsi.science, я (далее – «Пользователь» или «Субъект персональных данных») даю согласие на обработку персональных данных на этом сайте (текст Согласия) и на обработку персональных данных с помощью сервиса «Яндекс.Метрика» (текст Согласия).