Evaluating the Microhardness of Samples Based on Binder VST-1210 Cured under Various Conditions as a Method of Testing


Cite item

Full Text

Open Access Open Access
Restricted Access Access granted
Restricted Access Subscription Access

Abstract

Using a PMT-3M microhardness tester, the microhardness values depending on the distance of the spot of measurement from the frontal plane of the sample to its middle part are determined on the transverse sections of samples of binder VST-1210 hardened under various conditions. It is established that the microhardness value of a plastic depends on the conditions of its curing and also on the spot at which the measurement is carried out—the closer the sample core to the spot of measurement, the higher the microhardness value. The performed sclerometric tests have shown that the width of the groove trace also increases from the middle to the frontal plane of the sample.

About the authors

E. A. Veshkin

Ul’yanovsk Science and Technology Center, All-Russian Institute of Aviation Materials

Author for correspondence.
Email: untcviam@viam.ru
Russian Federation, Ul’yanovsk

V. I. Postnov

Ul’yanovsk Science and Technology Center, All-Russian Institute of Aviation Materials

Email: untcviam@viam.ru
Russian Federation, Ul’yanovsk

V. V. Semenychev

Ul’yanovsk Science and Technology Center, All-Russian Institute of Aviation Materials

Email: untcviam@viam.ru
Russian Federation, Ul’yanovsk


Copyright (c) 2019 Pleiades Publishing, Ltd.

This website uses cookies

You consent to our cookies if you continue to use our website.

About Cookies