Study of Local (Pitting) Wear of the Periclase-Carbon Lining of a Ladle
- Authors: Ryabyi D.V.1, Kondrukevich A.A.2
-
Affiliations:
- Donetsk National Technical University
- Russian University of Chemical Technology
- Issue: Vol 57, No 1 (2016)
- Pages: 4-5
- Section: Article
- URL: https://journals.rcsi.science/1083-4877/article/view/248132
- DOI: https://doi.org/10.1007/s11148-016-9915-8
- ID: 248132
Cite item
Abstract
Astudy is made of local (pitting) wear of the working layer of a periclase-carbon lining in a steel-pouring ladle used in a ladle-furnace unit without vacuum degassing of the steel that is being treated. The main causes of this type of wear are evaluated.
About the authors
D. V. Ryabyi
Donetsk National Technical University
Author for correspondence.
Email: Ryaboiy@gmail.com
Ukraine, Donetsk
A. A. Kondrukevich
Russian University of Chemical Technology
Email: Ryaboiy@gmail.com
Russian Federation, Moscow
Supplementary files