Magnetic chitosan microspheres were prepared by the emulsification cross-linking technique in the presence of glutaraldehyde as cross-linking agent, liquid paraffin as dispersant, and Span-80 as emulsifier. The optimal cross-linking time and Co0.5Ni0.5Fe2O4: chitosan ratio were determined. The morphology of particles was studied by different techniques. The adsorption characteristics were studied and the effect exerted by the initial concentration of methyl orange, the time of cross-linking, and the amount of the adsorbent was determined. It is found that the product obtained at the Co0.5Ni0.5Fe2O4: chitosan ratio 1: 4 and the crosslinking time 5 h has the uniform morphology. At room temperature, the Co0.5Ni0.5Fe2O4–chitosan magnetic composite has maximal adsorption for methyl orange at the dosage 20 mg.

Sobre autores

D. Jia

College of Chemical Engineering

Email: lianqilianqi517@163.com
República Popular da China, Qinhuangdao, 066600

D. Wang

Analysis and Testing Center

Email: lianqilianqi517@163.com
República Popular da China, Qinhuangdao, 066600

H. Wu

Chemical and Pharmaceutical Engineering

Email: lianqilianqi517@163.com
República Popular da China, Shijiazhuang, 050018

Q. Lian

College of Chemical Engineering

Autor responsável pela correspondência
Email: lianqilianqi517@163.com
República Popular da China, Qinhuangdao, 066600


Declaração de direitos autorais © Pleiades Publishing, Ltd., 2016

Este site utiliza cookies

Ao continuar usando nosso site, você concorda com o procedimento de cookies que mantêm o site funcionando normalmente.

Informação sobre cookies