Abrasive Wear Resistance of High-Speed Steel R6M5 after Laser Melting and Tempering
- Autores: Ratkevich G.V.1, Afanasieva L.E.1, Smolyakova I.A.1, Novoselova M.V.1
-
Afiliações:
- Tver State Technical University
- Edição: Volume 40, Nº 5 (2019)
- Páginas: 392-395
- Seção: Article
- URL: https://journals.rcsi.science/1068-3666/article/view/229330
- DOI: https://doi.org/10.3103/S106836661905012X
- ID: 229330
Citar
Resumo
This paper presents experimental studies of the microstructure, phase composition, microhardness distribution, estimation of abrasive wear resistance of rapid steel, grade R6M5, after laser melting and subsequent tempering. A multichannel (40 beams) CO2 laser was used to process the steel. It has been demonstrated that improved abrasive wear resistance is achieved after laser melt quenching and short-term tempering at 560°C.
Palavras-chave
Sobre autores
G. Ratkevich
Tver State Technical University
Email: ludmila.a@mail.ru
Rússia, Tver, 170026
L. Afanasieva
Tver State Technical University
Autor responsável pela correspondência
Email: ludmila.a@mail.ru
Rússia, Tver, 170026
I. Smolyakova
Tver State Technical University
Email: ludmila.a@mail.ru
Rússia, Tver, 170026
M. Novoselova
Tver State Technical University
Email: ludmila.a@mail.ru
Rússia, Tver, 170026
Arquivos suplementares