Synthesis of Microcrystals of Heavy-Boron-Doped Diamond and BC3-Heterodiamonds at High Pressures and Temperatures


如何引用文章

全文:

开放存取 开放存取
受限制的访问 ##reader.subscriptionAccessGranted##
受限制的访问 订阅存取

详细

The results of the synthesis and analysis of diamond crystals with heavy boron doping (about 2%), which were obtained from mixtures of gas black with m-carborane at 8 GPa and 1873 K, are presented. A high boron concentration in the diamond lattice was confirmed by x-ray data and the characteristic Raman scattering spectra, which correspond to diamond with metallic conductivity. Thermobaric treatment of the diamond-like dl-BC3 phase (1100 K, 25 GPa) results in the formation of BC3-heteronanodiamond.

作者简介

P. Zinin

Scientific and Technological Center for Unique Instrument Building, Russian Academy of Sciences

编辑信件的主要联系方式.
Email: zosimpvz@mail.ru
俄罗斯联邦, Moscow

V. Filonenko

Vereshchagin Institute of High-Pressure Physics, Russian Academy of Sciences

Email: zosimpvz@mail.ru
俄罗斯联邦, Troitsk

I. Zibrov

Vereshchagin Institute of High-Pressure Physics, Russian Academy of Sciences

Email: zosimpvz@mail.ru
俄罗斯联邦, Troitsk

A. Anokhin

A. A. Baikov Institute of Metallurgy and Materials Science, Russian Academy of Sciences

Email: zosimpvz@mail.ru
俄罗斯联邦, Moscow

E. Kukueva

National Research Center – Kurchatov Institute

Email: zosimpvz@mail.ru
俄罗斯联邦, Moscow

S. Lyapin

Vereshchagin Institute of High-Pressure Physics, Russian Academy of Sciences

Email: zosimpvz@mail.ru
俄罗斯联邦, Troitsk

I. Kutuza

Scientific and Technological Center for Unique Instrument Building, Russian Academy of Sciences

Email: zosimpvz@mail.ru
俄罗斯联邦, Moscow

补充文件

附件文件
动作
1. JATS XML

版权所有 © Springer Science+Business Media, LLC, part of Springer Nature, 2019