The results of the synthesis and analysis of diamond crystals with heavy boron doping (about 2%), which were obtained from mixtures of gas black with m-carborane at 8 GPa and 1873 K, are presented. A high boron concentration in the diamond lattice was confirmed by x-ray data and the characteristic Raman scattering spectra, which correspond to diamond with metallic conductivity. Thermobaric treatment of the diamond-like dl-BC3 phase (1100 K, 25 GPa) results in the formation of BC3-heteronanodiamond.

Авторлар туралы

P. Zinin

Scientific and Technological Center for Unique Instrument Building, Russian Academy of Sciences

Хат алмасуға жауапты Автор.
Email: zosimpvz@mail.ru
Ресей, Moscow

V. Filonenko

Vereshchagin Institute of High-Pressure Physics, Russian Academy of Sciences

Email: zosimpvz@mail.ru
Ресей, Troitsk

I. Zibrov

Vereshchagin Institute of High-Pressure Physics, Russian Academy of Sciences

Email: zosimpvz@mail.ru
Ресей, Troitsk

A. Anokhin

A. A. Baikov Institute of Metallurgy and Materials Science, Russian Academy of Sciences

Email: zosimpvz@mail.ru
Ресей, Moscow

E. Kukueva

National Research Center – Kurchatov Institute

Email: zosimpvz@mail.ru
Ресей, Moscow

S. Lyapin

Vereshchagin Institute of High-Pressure Physics, Russian Academy of Sciences

Email: zosimpvz@mail.ru
Ресей, Troitsk

I. Kutuza

Scientific and Technological Center for Unique Instrument Building, Russian Academy of Sciences

Email: zosimpvz@mail.ru
Ресей, Moscow

Қосымша файлдар

Қосымша файлдар
Әрекет
1. JATS XML

© Springer Science+Business Media, LLC, part of Springer Nature, 2019