Optimal Cooling Rate of Porous Fill Based on Liquid-Glass Compositions
- Authors: Abdrakhimova E.S.1
-
Affiliations:
- S. P. Korolev National Research University
- Issue: Vol 75, No 9-10 (2019)
- Pages: 366-369
- Section: Wastes into Production
- URL: https://journals.rcsi.science/0361-7610/article/view/245305
- DOI: https://doi.org/10.1007/s10717-019-00086-6
- ID: 245305
Cite item
Abstract
The composition and a method of production are proposed for high-porosity materials in low-temperature foaming of liquid glass and ash-slag material from burning of combustible shales used as fill and consumable additives. It is shown that keramzit based on liquid glass must be cooled at the rate 60 K/min, because a porous material with high structural quality factor and with high FeO content is formed at this cooling rate.