Optimal Cooling Rate of Porous Fill Based on Liquid-Glass Compositions


如何引用文章

全文:

开放存取 开放存取
受限制的访问 ##reader.subscriptionAccessGranted##
受限制的访问 订阅存取

详细

The composition and a method of production are proposed for high-porosity materials in low-temperature foaming of liquid glass and ash-slag material from burning of combustible shales used as fill and consumable additives. It is shown that keramzit based on liquid glass must be cooled at the rate 60 K/min, because a porous material with high structural quality factor and with high FeO content is formed at this cooling rate.