Gelation, Phase-Formation, and Sintering Processes in the Sol-Gel Method of Producing Aluminosilicate Glass-Ceramic Modified by Refractory Hafnium and Zirconium Oxides


如何引用文章

全文:

开放存取 开放存取
受限制的访问 ##reader.subscriptionAccessGranted##
受限制的访问 订阅存取

详细

Glass-ceramic based on compositions in the system Sr(Ba)–Al2O3–SiO2, modified by additions of zirconium oxide ZrO2 and hafnium oxide HfO2 with and without yttrium as a stabilizer, was synthesized by the sol-gel method. It was shown that the introduction of refractory oxides shortens the gelation time of the initial solutions, intensifies the sintering of the glass-ceramic, and changes the temperature intervals of phase formation processes and the nature of the precipitated crystalline phases. The sol-gel method made it possible to obtain a uniform distribution of the modifier-oxide grains in the bulk of the glass-ceramic. The yttrium oxide in the structure of the materials is concentrated near ZrO2 and HfO2 particles.

作者简介

A. Chainikova

All-Russia Scientific-Research Institute of Aviation Materials

编辑信件的主要联系方式.
Email: anna-chanikova@mail.ru
俄罗斯联邦, Moscow

V. Kovaleva

All-Russia Scientific-Research Institute of Aviation Materials

Email: anna-chanikova@mail.ru
俄罗斯联邦, Moscow

D. Zabelin

All-Russia Scientific-Research Institute of Aviation Materials

Email: anna-chanikova@mail.ru
俄罗斯联邦, Moscow

I. Belyachenkov

All-Russia Scientific-Research Institute of Aviation Materials

Email: anna-chanikova@mail.ru
俄罗斯联邦, Moscow

补充文件

附件文件
动作
1. JATS XML

版权所有 © Springer Science+Business Media, LLC, part of Springer Nature, 2019