Protective technological coatings for low-temperature deformation of semi-finished products and products from hard-to-deform alloys (titanium, zirconium, etc.) are considered. The process of low-temperature isometric product deformation made of the VT6 alloy, friction, and the separating properties of protective technological coatings are studied by compression of ring samples. Laboratory studies and industrial tests of pilot batches of coatings are carried out. Recommendations on the use of protective technological coatings are presented

Sobre autores

S. Polyanskii

Innovative Technologies Company, LLC

Email: psn50@mail.ru
620033, Yekaterinburg, Russia

S. Butakov

Yeltsin Ural Federal University

Email: psn50@mail.ru
620002, Yekaterinburg, Russia

A. Antimonov

Yeltsin Ural Federal University

Email: psn50@mail.ru
620002, Yekaterinburg, Russia

I. Ol’kov

Yeltsin Ural Federal University

Email: psn50@mail.ru
620002, Yekaterinburg, Russia

V. Aleksandrov

Ural State Agrarian University

Autor responsável pela correspondência
Email: psn50@mail.ru
620075, Yekaterinburg, Russia

Bibliografia

  1. Avitzur B. Handbook of metal-forming processes. New York: Wiley, 1983. 1020 p.
  2. Хайнике Г. Трибохимия. Пер. с англ. М.: Мир, 1987. 584 с.
  3. Кокрофт М.Г. Смазка в процессах обработки металлов давлением. М.: Металлургия, 1970. 111 с.
  4. Солнцев С.С. Защитные покрытия металлов при нагреве. Справочное пособие. Изд. 2, доп. М.: URSS, 2009. 248 с.
  5. Манегин Ю.В., Анисимова И.В. Стеклосмазки и защитные покрытия для горячей обработки металлов. М.: Металлургия, 1978. 224 с.
  6. Sejournet J. US Patent 3039888. Method of Coating the Bore of a Heated Hollow, 1966.
  7. Standard BAE APB 3 – 1108. British Aerospace PLC. Protective coating. GB, 1993. Iss. 1. 10 c.
  8. Zhu Y., Zeng W., Ma X., Tai Q., Li Z., Li X. Determination of the friction factor of Ti-6Al-4V titanium alloy in hot forging by means of ring-compression test using FEM // Tribology Int. 2011. V. 44 (12). P. 2074.
  9. Male A.T. Friction measurement using the ring compression test // In Proceedings of the Seventh ICTP Conf. 1, 2002. P. 321.
  10. Martin F. et al. The Ring Compression Test: Analysis of Dimensions and Canonical Geometry // Procedia Engineering. 2015. V. 132. P. 326.
  11. Rajesh E., SivaPrakash M. Analysis of friction factor by employing the ring compression test under different lubricants // Int. J. of Scientific & Engineering Research. 2013. V. 4. Iss. 5. P. 1163.
  12. Galdos L. et al. Characterization of Ti64 forging friction factor using ceramic coatings and different contact conditions // Procedia Engineering. 2017. V. 207. P. 2239.
  13. Li L.X., Peng D.S., Liu J.A., Liu Z.Q. An experiment study of the lubrication behavior of graphite in hot compression tests of Ti–6Al–4V alloy // J. of Materials Processing Technology. 2001. V. 112 (1). P. 1.

Arquivos suplementares

Arquivos suplementares
Ação
1. JATS XML
2.

Baixar (127KB)
3.

Baixar (17KB)
4.

Baixar (804KB)
5.

Baixar (23KB)

Declaração de direitos autorais © С.Н. Полянский, С.В. Бутаков, А.М. Антимонов, И.С. Ольков, В.А. Александров, 2023

Este site utiliza cookies

Ao continuar usando nosso site, você concorda com o procedimento de cookies que mantêm o site funcionando normalmente.

Informação sobre cookies