Evolution of the structure and mechanical properties of a bulk-nitrided corrosion-resistant ferritic steel upon tempering in the temperature range of 400–700°C


Дәйексөз келтіру

Толық мәтін

Ашық рұқсат Ашық рұқсат
Рұқсат жабық Рұқсат берілді
Рұқсат жабық Тек жазылушылар үшін

Аннотация

Methods of the X-ray diffraction analysis and electron microscopy were used to study changes in the structural phase state and mechanical properties of bulk-nitrided 08Kh17T steel (0.08 wt % C, 17 wt % Cr, 0.8 wt % Ti, 0.5 wt % Si, 0.8 wt % Mn, 0.025 wt % S, and 0.035 wt % P) upon tempering in the temperature range of 400–700°C. The changes in the mechanical properties of the nitrided steel upon tempering are associated with the predominance of either the solid-solution or precipitation strengthening, i.e., with the presence of martensite in the steel structure at low temperatures of tempering and the precipitation of particles of Cr2N nitrides of different dispersity upon increasing the tempering temperature. The greatest increase in the ultimate tensile strength and yield stress (1.8–2.5 times) at a satisfactory plasticity (no less than 10%) of the bulk-nitrided steel is achieved by tempering bulk-nitrided steel in a temperature range of 600–700°C.

Негізгі сөздер

Авторлар туралы

S. Rogachev

National University of Science and Technology MISiS

Хат алмасуға жауапты Автор.
Email: csaap@mail.ru
Ресей, Leninskii pr. 3, Moscow, 119049

S. Nikulin

National University of Science and Technology MISiS

Email: csaap@mail.ru
Ресей, Leninskii pr. 3, Moscow, 119049

V. Khatkevich

National University of Science and Technology MISiS

Email: csaap@mail.ru
Ресей, Leninskii pr. 3, Moscow, 119049


© Pleiades Publishing, Ltd., 2017

Осы сайт cookie-файлдарды пайдаланады

Біздің сайтты пайдалануды жалғастыра отырып, сіз сайттың дұрыс жұмыс істеуін қамтамасыз ететін cookie файлдарын өңдеуге келісім бересіз.< / br>< / br>cookie файлдары туралы< / a>