Analysis of the Causes of Failure of a Pipeline Welded Joint


如何引用文章

全文:

开放存取 开放存取
受限制的访问 ##reader.subscriptionAccessGranted##
受限制的访问 订阅存取

详细

An annular welded joint of a pipeline from steel 17G1S with diameter 1020 mm transporting natural gas at a pressure of 5.5 MPa is studied. The residual welding stresses are determined after failure of the pipes. Results of a study of fracture surfaces and of a metallographic analysis of the region of the welding defect over which the fracture has developed are presented. Mechanical tests of the pipe metal and of the metal of the welded joint are performed. The causes of failure of the joint are considered and methods for raising the reliability of pipelines are recommended.

作者简介

Yu. Chirkov

Orenburg State University (OSU)

编辑信件的主要联系方式.
Email: chircovura@mail.ru
俄罗斯联邦, Orenburg

V. Kushnarenko

Orenburg State University (OSU)

Email: chircovura@mail.ru
俄罗斯联邦, Orenburg

V. Repyakh

Orenburg State University (OSU)

Email: chircovura@mail.ru
俄罗斯联邦, Orenburg

E. Chirkov

“Tekhnopark OSU”

Email: chircovura@mail.ru
俄罗斯联邦, Orenburg

补充文件

附件文件
动作
1. JATS XML

版权所有 © Springer Science+Business Media, LLC, part of Springer Nature, 2018