Silicidation of Tantalum Carbide and Zirconium Carbide Powders in a Gaseous SiO Environment
- Авторы: Belyaev I.M.1, Istomin P.V.1, Istomina E.I.1
-
Учреждения:
- Institute of Chemistry, Komi Scientific Center, Ural Branch
- Выпуск: Том 54, № 8 (2018)
- Страницы: 779-786
- Раздел: Article
- URL: https://journals.rcsi.science/0020-1685/article/view/158501
- DOI: https://doi.org/10.1134/S0020168518080022
- ID: 158501
Цитировать
Аннотация
Tantalum carbide and zirconium carbide powders have been silicided in a gaseous SiO atmosphere at 1400°C. X-ray diffraction and energy dispersive X-ray microanalysis results demonstrate that the silicidation products are Ta5Si3 and TaSi2 in the case of TaC and ZrSi in the case of ZrC. The silicidation rate has been shown to influence the percentages of these silicides in the reaction products. The degree of silicidation reached in this study is about 20% in the case of TaC and about 16% in the case of ZrC.
Ключевые слова
Об авторах
I. Belyaev
Institute of Chemistry, Komi Scientific Center, Ural Branch
Email: istomin-pv@yandex.ru
Россия, Pervomaiskaya ul. 48, Syktyvkar, Komi Republic, 167000
P. Istomin
Institute of Chemistry, Komi Scientific Center, Ural Branch
Автор, ответственный за переписку.
Email: istomin-pv@yandex.ru
Россия, Pervomaiskaya ul. 48, Syktyvkar, Komi Republic, 167000
E. Istomina
Institute of Chemistry, Komi Scientific Center, Ural Branch
Email: istomin-pv@yandex.ru
Россия, Pervomaiskaya ul. 48, Syktyvkar, Komi Republic, 167000
Дополнительные файлы