Silicidation of Tantalum Carbide and Zirconium Carbide Powders in a Gaseous SiO Environment


如何引用文章

全文:

开放存取 开放存取
受限制的访问 ##reader.subscriptionAccessGranted##
受限制的访问 订阅存取

详细

Tantalum carbide and zirconium carbide powders have been silicided in a gaseous SiO atmosphere at 1400°C. X-ray diffraction and energy dispersive X-ray microanalysis results demonstrate that the silicidation products are Ta5Si3 and TaSi2 in the case of TaC and ZrSi in the case of ZrC. The silicidation rate has been shown to influence the percentages of these silicides in the reaction products. The degree of silicidation reached in this study is about 20% in the case of TaC and about 16% in the case of ZrC.

作者简介

I. Belyaev

Institute of Chemistry, Komi Scientific Center, Ural Branch

Email: istomin-pv@yandex.ru
俄罗斯联邦, Pervomaiskaya ul. 48, Syktyvkar, Komi Republic, 167000

P. Istomin

Institute of Chemistry, Komi Scientific Center, Ural Branch

编辑信件的主要联系方式.
Email: istomin-pv@yandex.ru
俄罗斯联邦, Pervomaiskaya ul. 48, Syktyvkar, Komi Republic, 167000

E. Istomina

Institute of Chemistry, Komi Scientific Center, Ural Branch

Email: istomin-pv@yandex.ru
俄罗斯联邦, Pervomaiskaya ul. 48, Syktyvkar, Komi Republic, 167000

补充文件

附件文件
动作
1. JATS XML

版权所有 © Pleiades Publishing, Ltd., 2018