Strength of display glass
- Авторлар: Baikova L.G.1, Kireenko M.F.1, Pesina T.I.1, Startsev Y.K.1, Tikhonova L.V.1
-
Мекемелер:
- Ioffe Physical and Technical Institute
- Шығарылым: Том 42, № 5 (2016)
- Беттер: 449-452
- Бөлім: Article
- URL: https://journals.rcsi.science/1087-6596/article/view/215685
- DOI: https://doi.org/10.1134/S1087659616050035
- ID: 215685
Дәйексөз келтіру
Аннотация
The strength of dual-display glass surfaces 0.64 mm (Corning 1737 glass) and 0.70 mm (Eagle2000 glass) thick is measured in the initial state and after annealing. Large dispersion of the strength of the glass before and after annealing is found. It is suggested that the low values of the strength are caused by the adverse conditions of storing and handling glass samples.
Негізгі сөздер
Авторлар туралы
L. Baikova
Ioffe Physical and Technical Institute
Хат алмасуға жауапты Автор.
Email: lgbaikova@gmail.com
Ресей, St. Petersburg, 194021
M. Kireenko
Ioffe Physical and Technical Institute
Email: lgbaikova@gmail.com
Ресей, St. Petersburg, 194021
T. Pesina
Ioffe Physical and Technical Institute
Email: lgbaikova@gmail.com
Ресей, St. Petersburg, 194021
Yu. Startsev
Ioffe Physical and Technical Institute
Email: lgbaikova@gmail.com
Ресей, St. Petersburg, 194021
L. Tikhonova
Ioffe Physical and Technical Institute
Email: lgbaikova@gmail.com
Ресей, St. Petersburg, 194021
Қосымша файлдар