The strength of dual-display glass surfaces 0.64 mm (Corning 1737 glass) and 0.70 mm (Eagle2000 glass) thick is measured in the initial state and after annealing. Large dispersion of the strength of the glass before and after annealing is found. It is suggested that the low values of the strength are caused by the adverse conditions of storing and handling glass samples.

Sobre autores

L. Baikova

Ioffe Physical and Technical Institute

Autor responsável pela correspondência
Email: lgbaikova@gmail.com
Rússia, St. Petersburg, 194021

M. Kireenko

Ioffe Physical and Technical Institute

Email: lgbaikova@gmail.com
Rússia, St. Petersburg, 194021

T. Pesina

Ioffe Physical and Technical Institute

Email: lgbaikova@gmail.com
Rússia, St. Petersburg, 194021

Yu. Startsev

Ioffe Physical and Technical Institute

Email: lgbaikova@gmail.com
Rússia, St. Petersburg, 194021

L. Tikhonova

Ioffe Physical and Technical Institute

Email: lgbaikova@gmail.com
Rússia, St. Petersburg, 194021

Arquivos suplementares

Arquivos suplementares
Ação
1. JATS XML

Declaração de direitos autorais © Pleiades Publishing, Ltd., 2016