Permeable Ceramic with Three-Fraction Electromelted Corundum Filler and Porcelain Binder


如何引用文章

全文:

开放存取 开放存取
受限制的访问 ##reader.subscriptionAccessGranted##
受限制的访问 订阅存取

详细

Porous permeable materials are prepared by selecting the grain size composition with electromelted corundum filler and porcelain mix PFL-1 binder. Specimens with an improved set of properties are prepared with addition to the composition of 5 wt.% porcelain binder (above 100% filler) after firing at 1450°C. Specimen ultimate strength in bending is 14.6 MPa, open porosity 44%, and gas permeability coefficient 0.85 μm2.

作者简介

A. Belyakov

D. I. Mendeleev Russian Chemical Technology University

编辑信件的主要联系方式.
Email: av_bel@bk.ru
俄罗斯联邦, Moscow

Zaw Oo

D. I. Mendeleev Russian Chemical Technology University

Email: av_bel@bk.ru
俄罗斯联邦, Moscow

N. Popova

D. I. Mendeleev Russian Chemical Technology University

Email: av_bel@bk.ru
俄罗斯联邦, Moscow

Ye Min

D. I. Mendeleev Russian Chemical Technology University

Email: av_bel@bk.ru
俄罗斯联邦, Moscow

补充文件

附件文件
动作
1. JATS XML

版权所有 © Springer Science+Business Media, LLC, part of Springer Nature, 2018