Highly Porous Granulated Corundum Filler of Alumina-Foam Polystyrene Mixture. Part 5. Effect of Molding Mixture Fineness and Moisture Content on Filler Granulation Capacity and Physicotechnical Properties1
- Авторы: Sokov V.N.1
-
Учреждения:
- FGBOU VO NIU Moscow State Building University
- Выпуск: Том 59, № 1 (2018)
- Страницы: 54-58
- Раздел: Article
- URL: https://journals.rcsi.science/1083-4877/article/view/248985
- DOI: https://doi.org/10.1007/s11148-018-0182-8
- ID: 248985
Цитировать
Аннотация
It is established that there are three stages in molding mixture pelletization: nucleus formation, granule growth, and mass transfer between them. Addition of a surfactant improves granulation capacity and reduces molding moisture content, and increases raw granule strength. The fineness of the starting material has a significant effect on capillary reaction forces that are fundamental during molding mixture pelletization.
Об авторах
V. Sokov
FGBOU VO NIU Moscow State Building University
Автор, ответственный за переписку.
Email: sersok_07@mail.ru
Россия, Moscow
Дополнительные файлы