A Study of the Electroerosive Wear of Surfaces of Accelerating Channels of a Coaxial Magnetoplasma Accelerator


如何引用文章

全文:

开放存取 开放存取
受限制的访问 ##reader.subscriptionAccessGranted##
受限制的访问 订阅存取

详细

Results of experimental studies of electroerosive wear of accelerating channels’ surface of coaxial magneto-plasma accelerator are presented. The main patterns of the accelerating channel electroerosive wear of titanium, stainless-steel, copper, and duralumin coaxial magnetoplasma accelerators (CMPAs) are determined. The optimum length of the accelerating channel in the range of delivered energy in the region of 50 kJ, wherein up to 90% of the material carried out by the hypersonic jet of electroerosion plasma is turned out, are determined. For titanium, stainless steel and duralumin barrels, it is about 150 mm and for a copper one it is 100 mm. The analytic expression allowing one to estimate the required weight value of eroded material with certain energy and structural parameters of CMPA are obtained on the base of experimental studies.

作者简介

A. Sivkov

National Research Polytechnic University

编辑信件的主要联系方式.
Email: journal-elektrotechnika@mail.ru
俄罗斯联邦, Tomsk, 634050

D. Gerasimov

National Research Polytechnic University

Email: journal-elektrotechnika@mail.ru
俄罗斯联邦, Tomsk, 634050

补充文件

附件文件
动作
1. JATS XML

版权所有 © Allerton Press, Inc., 2018