Decay of H2O2 under the action of the colloidal catalyst based on iron(III) oxides in a neutral medium


Дәйексөз келтіру

Толық мәтін

Ашық рұқсат Ашық рұқсат
Рұқсат жабық Рұқсат берілді
Рұқсат жабық Тек жазылушылар үшін

Аннотация

The catalytic activity of the colloidal catalyst based on iron(III) hydroxide was studied in the decomposition of H2O2 in a neutral medium (pH 6.7). A colloidal micellar solution of iron(III) hydroxide after preparation was kept at 19–20 °С for 2 or 20 h without additives or with C2H5OH additives. The decomposition of H2O2 under the action of the colloidal catalyst (20 h) proceeds via the first-order reaction with the decay rate constant kd = 1.26•10–4 s–1, whereas the decay rate of the first-order reaction is kd = 0.77•10–4 s–1 for the colloidal catalyst (2 h) prepared in the presence of C2H5OH.

Авторлар туралы

L. Pisarenko

N. N. Semenov Institute of Chemical Physics, Russian Academy of Sciences

Хат алмасуға жауапты Автор.
Email: pissarenkolm@mail.ru
Ресей, 4 ul. Kosygina, Moscow, 119991

Қосымша файлдар

Қосымша файлдар
Әрекет
1. JATS XML

© Springer Science+Business Media, LLC, part of Springer Nature, 2018