Structure of Relaxor Ferroelectric (1 – 2х)BiScO3 · хPbTiO3 · хPbMg0.33Nb0.67O3 with х = 0.42 in the Polarized and Depolarized States


Citar

Texto integral

Acesso aberto Acesso aberto
Acesso é fechado Acesso está concedido
Acesso é fechado Somente assinantes

Resumo

An X-ray diffraction study of ceramic samples of relaxor ferroelectric (1 – 2х)BiScO3 · хPbTiO3 · хPbMg0.33Nb0.67O3 with х = 0.42 in the polarized and depolarized states has been performed. It is established by Rietveld method that in both cases samples contain two perovskite-like phases, which are solid solutions. One of them has cubic symmetry. The second phase is characterized by the polar tetragonal sp. gr. P4mm in the polarized state and the monoclinic noncentrosymmetric sp. gr. Cm in the depolarized state.

Sobre autores

V. Sirotinkin

Moscow Technological University (MIREA)

Autor responsável pela correspondência
Email: sirotinkin.vladimir@mail.ru
Rússia, Moscow, 119454

A. Bush

Moscow Technological University (MIREA)

Email: sirotinkin.vladimir@mail.ru
Rússia, Moscow, 119454

A. Spitsin

ELPA Research Institute

Email: sirotinkin.vladimir@mail.ru
Rússia, Zelenograd, Moscow, 124460

A. Segalla

ELPA Research Institute

Email: sirotinkin.vladimir@mail.ru
Rússia, Zelenograd, Moscow, 124460

Arquivos suplementares

Arquivos suplementares
Ação
1. JATS XML

Declaração de direitos autorais © Pleiades Publishing, Inc., 2018