Crossover from an ordinary ferroelectric to a relaxor in Sr2 + xBi4–xTi5–xNbxO18
- Autores: Gridnev S.A.1, Tolstykh N.A.1, Bocharov A.I.1, Zhivotenko N.V.1
-
Afiliações:
- Voronezh State Technical University
- Edição: Volume 80, Nº 9 (2016)
- Páginas: 1064-1067
- Seção: Proceedings of the VIII (XIII) International Seminar on the Physics of Ferroelastics
- URL: https://journals.rcsi.science/1062-8738/article/view/184810
- DOI: https://doi.org/10.3103/S1062873816090161
- ID: 184810
Citar
Resumo
Sr2 + xBi4–xTi5–xNbxO18 materials with x = 0.2, 0.4, 0.6, 0.8, and 1 are synthesized. Investigations of the dielectric constant of the samples reveal an increase in the blurring of the phase transition as the share of titanium ions substituted for niobium ions grows. The Burns temperature and the temperature corresponding to the dielectric permittivity maximum are determined for all of the above compositions. Crossover from a normal ferroelectric to a relaxor ferroelectric in Sr2 + xBi4–xTi5–xNbxO18 samples is observed.
Sobre autores
S. Gridnev
Voronezh State Technical University
Email: mad_nik@bk.ru
Rússia, Voronezh, 394026
N. Tolstykh
Voronezh State Technical University
Autor responsável pela correspondência
Email: mad_nik@bk.ru
Rússia, Voronezh, 394026
A. Bocharov
Voronezh State Technical University
Email: mad_nik@bk.ru
Rússia, Voronezh, 394026
N. Zhivotenko
Voronezh State Technical University
Email: mad_nik@bk.ru
Rússia, Voronezh, 394026
Arquivos suplementares