Crossover from an ordinary ferroelectric to a relaxor in Sr2 + xBi4–xTi5–xNbxO18


Цитировать

Полный текст

Открытый доступ Открытый доступ
Доступ закрыт Доступ предоставлен
Доступ закрыт Только для подписчиков

Аннотация

Sr2 + xBi4–xTi5–xNbxO18 materials with x = 0.2, 0.4, 0.6, 0.8, and 1 are synthesized. Investigations of the dielectric constant of the samples reveal an increase in the blurring of the phase transition as the share of titanium ions substituted for niobium ions grows. The Burns temperature and the temperature corresponding to the dielectric permittivity maximum are determined for all of the above compositions. Crossover from a normal ferroelectric to a relaxor ferroelectric in Sr2 + xBi4–xTi5–xNbxO18 samples is observed.

Об авторах

S. Gridnev

Voronezh State Technical University

Email: mad_nik@bk.ru
Россия, Voronezh, 394026

N. Tolstykh

Voronezh State Technical University

Автор, ответственный за переписку.
Email: mad_nik@bk.ru
Россия, Voronezh, 394026

A. Bocharov

Voronezh State Technical University

Email: mad_nik@bk.ru
Россия, Voronezh, 394026

N. Zhivotenko

Voronezh State Technical University

Email: mad_nik@bk.ru
Россия, Voronezh, 394026

Дополнительные файлы

Доп. файлы
Действие
1. JATS XML

© Allerton Press, Inc., 2016

Согласие на обработку персональных данных

 

Используя сайт https://journals.rcsi.science, я (далее – «Пользователь» или «Субъект персональных данных») даю согласие на обработку персональных данных на этом сайте (текст Согласия) и на обработку персональных данных с помощью сервиса «Яндекс.Метрика» (текст Согласия).