Spark plasma sintering of β-SiAlON–BN composites from combustion-synthesized powders
- Authors: Nefedova E.V.1, Grigoryev E.G.1, Fokin D.A.1, Smirnov K.L.2
-
Affiliations:
- National Research Nuclear University MEPhI
- Institute of Structural Macrokinetics and Materials Science
- Issue: Vol 25, No 4 (2016)
- Pages: 229-233
- Section: Article
- URL: https://journals.rcsi.science/1061-3862/article/view/195756
- DOI: https://doi.org/10.3103/S1061386216040075
- ID: 195756
Cite item
Abstract
Investigated was the spark plasma sintering (SPS) of β-SiAlON/0–30 wt % BN ceramic composites. The raw materials (β-Si5AlON7 and BN powders) were prepared by infiltration-mediated combustion synthesis (CS). Experimentally established were the following process parameters for SPS of composites with high relative density (>95%) and flexural strength of 250–300 MPa: (a) heating rate 50 deg/min, (b) maximum temperature 1650–1750°C, (c) and holding time 5 min.
About the authors
E. V. Nefedova
National Research Nuclear University MEPhI
Email: kosm@ism.ac.ru
Russian Federation, Moscow, 115409
E. G. Grigoryev
National Research Nuclear University MEPhI
Email: kosm@ism.ac.ru
Russian Federation, Moscow, 115409
D. A. Fokin
National Research Nuclear University MEPhI
Email: kosm@ism.ac.ru
Russian Federation, Moscow, 115409
K. L. Smirnov
Institute of Structural Macrokinetics and Materials Science
Author for correspondence.
Email: kosm@ism.ac.ru
Russian Federation, Chernogolovka, Moscow, 142432
Supplementary files