Linear Thermal Expansion Coefficient (at Temperatures from 130 to 800 K) of Borosilicate Glasses Suitable for Silicon Compounds in Microelectronics


如何引用文章

全文:

开放存取 开放存取
受限制的访问 ##reader.subscriptionAccessGranted##
受限制的访问 订阅存取

详细

The measurements of the CLTE and relative elongation of two types of borosilicate glasses — LK5 and Borofloat 33 — are analyzed. A TMA7100 thermomechanical analyzer is used to measure the elongation of glass samples at temperatures from 130 to 800 K (−143 to +526°C). The relative error of indirect measurements of the CLTE and the relative thermal elongation of both types of glasses did not exceed ±5 and ±3%, respectively. Polynomial equations for obtaining fits to the measurements as a function of the temperature are presented. The results will facilitate the modeling of the characteristics of the devices which are used in microsystems engineering and fabricated by anodic deposition of silicon on glass; they can also be used to optimize the temperature regime of silicon bonding with glass.

作者简介

L. Sinev

N. L. Dukhov All-Russia Scientific-Research Institute of Automatics (VNIIA)

编辑信件的主要联系方式.
Email: leonid.sinev@yandex.ru
俄罗斯联邦, Moscow

I. Petrov

N. L. Dukhov All-Russia Scientific-Research Institute of Automatics (VNIIA)

Email: leonid.sinev@yandex.ru
俄罗斯联邦, Moscow

补充文件

附件文件
动作
1. JATS XML

版权所有 © Springer Science+Business Media New York, 2016