Calcium Phosphate Foam Ceramic Based on Hydroxyapatite–Brushite Powder Mixture


Citar

Texto integral

Acesso aberto Acesso aberto
Acesso é fechado Acesso está concedido
Acesso é fechado Somente assinantes

Resumo

The introduction of 10 – 50% (by weight) brushite powder, preheated at 50° and then fired at 1200°C, into a permeating suspension based on hydroxyapatite powder heat-treated at 800°C results in partial decomposition of hydroxyapatite to the α- and β-modifications of tricalcium phosphate. The presence of a tricalcium phosphate phase in calcium phosphate foam ceramic promotes an increase of the porosity from 40 to 60% and the resorption with significant static strength reduction from 3 – 7 to 0.3 MPa.

Sobre autores

V. Krut’ko

Institute of General and Inorganic Chemistry, National Academy of Sciences of Belarus

Autor responsável pela correspondência
Email: tsuber@igic.bas-net.by
Belarus, Minsk

A. Kulak

Institute of General and Inorganic Chemistry, National Academy of Sciences of Belarus

Email: tsuber@igic.bas-net.by
Belarus, Minsk

O. Musskaya

Institute of General and Inorganic Chemistry, National Academy of Sciences of Belarus

Email: tsuber@igic.bas-net.by
Belarus, Minsk

T. Safronova

M. V. Lomonosov Moscow State University

Email: tsuber@igic.bas-net.by
Rússia, Moscow

V. Putlyaev

M. V. Lomonosov Moscow State University

Email: tsuber@igic.bas-net.by
Rússia, Moscow

Arquivos suplementares

Arquivos suplementares
Ação
1. JATS XML

Declaração de direitos autorais © Springer Science+Business Media, LLC, part of Springer Nature, 2019