Production and Properties of Ceramic Obtained From Cobalt Oxide Nanopowder
- Authors: Lysenko V.I.1
-
Affiliations:
- S. A. Khristianovich Institute of Theoretical and Applied Mechanics
- Issue: Vol 74, No 3-4 (2017)
- Pages: 126-127
- Section: Article
- URL: https://journals.rcsi.science/0361-7610/article/view/244807
- DOI: https://doi.org/10.1007/s10717-017-9944-x
- ID: 244807
Cite item
Abstract
Spark plasma sintering (SPS) was used to obtain a fine-grain (of the order of 200 nm), dense, strong ceramic (microhardness to 10 GPa) on the basis of nanosize cobalt oxide powder.
About the authors
V. I. Lysenko
S. A. Khristianovich Institute of Theoretical and Applied Mechanics
Author for correspondence.
Email: vl@itam.nsc.ru
Russian Federation, Novosibirsk
Supplementary files