Estimation of the Delayed Hydride Cracking Resistance of the Pressure Tubes in Nuclear Reactors
- 作者: Shmakov A.1, Singh R.2, Matvienko Y.3, Kolmakov A.4
-
隶属关系:
- National University of Science and Technology MISiS
- Atomic Research Center
- IMASh RAN
- IMET RAN
- 期: 卷 2018, 编号 4 (2018)
- 页面: 397-401
- 栏目: Applied Problems of Strength and Plasticity
- URL: https://journals.rcsi.science/0036-0295/article/view/172498
- DOI: https://doi.org/10.1134/S0036029518040146
- ID: 172498
如何引用文章
详细
The resistances of the pressure tubes in pressure tube reactors to fracture according to the delayed hydride cracking mechanism are compared. The allowable cracklike defect sizes in the pressure tubes of CANDU, IPHWR, and RBMK-1000 rectors are calculated. These results can be used to ground the service reserve of Zr–2.5% Nb alloy reactor tubes.
作者简介
A. Shmakov
National University of Science and Technology MISiS
Email: matvienko7@yahoo.com
俄罗斯联邦, Moscow, 119049
R. Singh
Atomic Research Center
Email: matvienko7@yahoo.com
印度, Mumbai, 400085
Yu. Matvienko
IMASh RAN
编辑信件的主要联系方式.
Email: matvienko7@yahoo.com
俄罗斯联邦, Moscow, 101990
A. Kolmakov
IMET RAN
Email: matvienko7@yahoo.com
俄罗斯联邦, Moscow, 119334
![](/img/style/loading.gif)