Metallization of siderite ore in reducing roasting
- 作者: Gulyakov V.1, Vusikhis A.1, Leont’ev L.1, Kudinov D.1
-
隶属关系:
- Institute of Metallurgy, Ural Branch
- 期: 卷 2016, 编号 5 (2016)
- 页面: 404-408
- 栏目: Article
- URL: https://journals.rcsi.science/0036-0295/article/view/170513
- DOI: https://doi.org/10.1134/S0036029516050153
- ID: 170513
如何引用文章
详细
The behavior of the initial ore and the concentrate of magnetoroasting beneficiation during metallization under the conditions that are close to those for reducing roasting of iron ores in a rotary furnace is studied in terms of works on extending the field of application of Bakal siderites. A difference in the mechanisms of the metallization of crude ore and the roasted concentrate is observed. The metallization of roasted concentrate lumps is more efficient than that of crude siderite ore. In this case, the process ends earlier and can be carried out at higher temperatures (1250–1300°C) without danger of skull formation.
作者简介
V. Gulyakov
Institute of Metallurgy, Ural Branch
Email: vas58@mail.ru
俄罗斯联邦, ul. Amundsena 101, Yekaterinburg, 620016
A. Vusikhis
Institute of Metallurgy, Ural Branch
编辑信件的主要联系方式.
Email: vas58@mail.ru
俄罗斯联邦, ul. Amundsena 101, Yekaterinburg, 620016
L. Leont’ev
Institute of Metallurgy, Ural Branch
Email: vas58@mail.ru
俄罗斯联邦, ul. Amundsena 101, Yekaterinburg, 620016
D. Kudinov
Institute of Metallurgy, Ural Branch
Email: vas58@mail.ru
俄罗斯联邦, ul. Amundsena 101, Yekaterinburg, 620016
![](/img/style/loading.gif)