The behavior of the initial ore and the concentrate of magnetoroasting beneficiation during metallization under the conditions that are close to those for reducing roasting of iron ores in a rotary furnace is studied in terms of works on extending the field of application of Bakal siderites. A difference in the mechanisms of the metallization of crude ore and the roasted concentrate is observed. The metallization of roasted concentrate lumps is more efficient than that of crude siderite ore. In this case, the process ends earlier and can be carried out at higher temperatures (1250–1300°C) without danger of skull formation.

Авторлар туралы

V. Gulyakov

Institute of Metallurgy, Ural Branch

Email: vas58@mail.ru
Ресей, ul. Amundsena 101, Yekaterinburg, 620016

A. Vusikhis

Institute of Metallurgy, Ural Branch

Хат алмасуға жауапты Автор.
Email: vas58@mail.ru
Ресей, ul. Amundsena 101, Yekaterinburg, 620016

L. Leont’ev

Institute of Metallurgy, Ural Branch

Email: vas58@mail.ru
Ресей, ul. Amundsena 101, Yekaterinburg, 620016

D. Kudinov

Institute of Metallurgy, Ural Branch

Email: vas58@mail.ru
Ресей, ul. Amundsena 101, Yekaterinburg, 620016


© Pleiades Publishing, Ltd., 2016

Осы сайт cookie-файлдарды пайдаланады

Біздің сайтты пайдалануды жалғастыра отырып, сіз сайттың дұрыс жұмыс істеуін қамтамасыз ететін cookie файлдарын өңдеуге келісім бересіз.< / br>< / br>cookie файлдары туралы< / a>