Metallization of siderite ore in reducing roasting


Цитировать

Полный текст

Открытый доступ Открытый доступ
Доступ закрыт Доступ предоставлен
Доступ закрыт Только для подписчиков

Аннотация

The behavior of the initial ore and the concentrate of magnetoroasting beneficiation during metallization under the conditions that are close to those for reducing roasting of iron ores in a rotary furnace is studied in terms of works on extending the field of application of Bakal siderites. A difference in the mechanisms of the metallization of crude ore and the roasted concentrate is observed. The metallization of roasted concentrate lumps is more efficient than that of crude siderite ore. In this case, the process ends earlier and can be carried out at higher temperatures (1250–1300°C) without danger of skull formation.

Об авторах

V. Gulyakov

Institute of Metallurgy, Ural Branch

Email: vas58@mail.ru
Россия, ul. Amundsena 101, Yekaterinburg, 620016

A. Vusikhis

Institute of Metallurgy, Ural Branch

Автор, ответственный за переписку.
Email: vas58@mail.ru
Россия, ul. Amundsena 101, Yekaterinburg, 620016

L. Leont’ev

Institute of Metallurgy, Ural Branch

Email: vas58@mail.ru
Россия, ul. Amundsena 101, Yekaterinburg, 620016

D. Kudinov

Institute of Metallurgy, Ural Branch

Email: vas58@mail.ru
Россия, ul. Amundsena 101, Yekaterinburg, 620016


© Pleiades Publishing, Ltd., 2016

Данный сайт использует cookie-файлы

Продолжая использовать наш сайт, вы даете согласие на обработку файлов cookie, которые обеспечивают правильную работу сайта.

О куки-файлах