Forces and strains during drop weight tear test


Цитировать

Полный текст

Открытый доступ Открытый доступ
Доступ закрыт Доступ предоставлен
Доступ закрыт Только для подписчиков

Аннотация

As follows from the results of drop weight tear tests (DWTT), modern strength class K65 steels for gas-main pipelines exhibit an almost 100% fraction of ductile component in a fracture surface. The results of ground tests demonstrate that the lengths of extended fracture of a pipe made of such steels from different suppliers are substantially different. The possibility of extracting other characteristics from DWTT tests of full-thickness notched specimens and the information content in them are estimated. High-speed detection of the strain and crack growth is performed during static and dynamic loading. As follows from an analysis of fracture kinematics and force and energy balance, fracture is a multistage process, where mechanisms change during crack growth.

Об авторах

M. Shtremel’

NITU MISiS

Автор, ответственный за переписку.
Email: str@mfp.misis.ru
Россия, Moscow, 119991

A. Arabei

PAO Gazprom

Email: str@mfp.misis.ru
Россия, Moscow, 117997

A. Glebov

NITU MISiS

Email: str@mfp.misis.ru
Россия, Moscow, 119991

A. Abakumov

FGUP RFYaTs-VNIIEF

Email: str@mfp.misis.ru
Россия, Sarov, 607188

T. Esiev

OOO Gasprom VNIIGAZ

Email: str@mfp.misis.ru
Россия, Moscow, 115583

A. Struin

OAO PosNITI

Email: str@mfp.misis.ru
Россия, Chelyabinsk, 454139

B. Sarychev

OAO MMK

Email: str@mfp.misis.ru
Россия, Magnitogorsk, 455019

Дополнительные файлы

Доп. файлы
Действие
1. JATS XML

© Pleiades Publishing, Ltd., 2017

Согласие на обработку персональных данных

 

Используя сайт https://journals.rcsi.science, я (далее – «Пользователь» или «Субъект персональных данных») даю согласие на обработку персональных данных на этом сайте (текст Согласия) и на обработку персональных данных с помощью сервиса «Яндекс.Метрика» (текст Согласия).