As follows from the results of drop weight tear tests (DWTT), modern strength class K65 steels for gas-main pipelines exhibit an almost 100% fraction of ductile component in a fracture surface. The results of ground tests demonstrate that the lengths of extended fracture of a pipe made of such steels from different suppliers are substantially different. The possibility of extracting other characteristics from DWTT tests of full-thickness notched specimens and the information content in them are estimated. High-speed detection of the strain and crack growth is performed during static and dynamic loading. As follows from an analysis of fracture kinematics and force and energy balance, fracture is a multistage process, where mechanisms change during crack growth.

Авторлар туралы

M. Shtremel’

NITU MISiS

Хат алмасуға жауапты Автор.
Email: str@mfp.misis.ru
Ресей, Moscow, 119991

A. Arabei

PAO Gazprom

Email: str@mfp.misis.ru
Ресей, Moscow, 117997

A. Glebov

NITU MISiS

Email: str@mfp.misis.ru
Ресей, Moscow, 119991

A. Abakumov

FGUP RFYaTs-VNIIEF

Email: str@mfp.misis.ru
Ресей, Sarov, 607188

T. Esiev

OOO Gasprom VNIIGAZ

Email: str@mfp.misis.ru
Ресей, Moscow, 115583

A. Struin

OAO PosNITI

Email: str@mfp.misis.ru
Ресей, Chelyabinsk, 454139

B. Sarychev

OAO MMK

Email: str@mfp.misis.ru
Ресей, Magnitogorsk, 455019


© Pleiades Publishing, Ltd., 2017

Осы сайт cookie-файлдарды пайдаланады

Біздің сайтты пайдалануды жалғастыра отырып, сіз сайттың дұрыс жұмыс істеуін қамтамасыз ететін cookie файлдарын өңдеуге келісім бересіз.< / br>< / br>cookie файлдары туралы< / a>