Changes in the Defect Structure of the Pd–5.3 at % In–0.5 at % Ru Alloy Subjected to Electrolytic Hydrogenation and Prolonged Relaxation
- 作者: Akimova O.V.1, Avdyukhina V.M.1, Shchetinin I.V.2
-
隶属关系:
- Physical Department
- National University of Science and Technology MISIS
- 期: 卷 117, 编号 3 (2016)
- 页面: 275-278
- 栏目: Structure, Phase Transformations, and Diffusion
- URL: https://journals.rcsi.science/0031-918X/article/view/166666
- DOI: https://doi.org/10.1134/S0031918X16030017
- ID: 166666
如何引用文章
详细
Variations in the reduced integral intensities of diffraction maxima in X-ray diffraction patterns taken for the Pd–5.3 at % In–0.5 at % Ru alloy foil, which was subjected to electrolytic saturation with hydrogen and subsequent prolonged relaxation at room temperature and atmospheric pressure, have been analyzed. The degree of texture of the sample has been found to decrease substantially, and first-class defects in the alloy matrix dominate.
作者简介
O. Akimova
Physical Department
编辑信件的主要联系方式.
Email: akimova@physics.msu.ru
俄罗斯联邦, Leninskie Gory 1, build. 2, Moscow, 119991
V. Avdyukhina
Physical Department
Email: akimova@physics.msu.ru
俄罗斯联邦, Leninskie Gory 1, build. 2, Moscow, 119991
I. Shchetinin
National University of Science and Technology MISIS
Email: akimova@physics.msu.ru
俄罗斯联邦, Leninskii pr. 4, Moscow, 119049
补充文件