Changes in the Defect Structure of the Pd–5.3 at % In–0.5 at % Ru Alloy Subjected to Electrolytic Hydrogenation and Prolonged Relaxation
- Авторы: Akimova O.V.1, Avdyukhina V.M.1, Shchetinin I.V.2
-
Учреждения:
- Physical Department
- National University of Science and Technology MISIS
- Выпуск: Том 117, № 3 (2016)
- Страницы: 275-278
- Раздел: Structure, Phase Transformations, and Diffusion
- URL: https://journals.rcsi.science/0031-918X/article/view/166666
- DOI: https://doi.org/10.1134/S0031918X16030017
- ID: 166666
Цитировать
Аннотация
Variations in the reduced integral intensities of diffraction maxima in X-ray diffraction patterns taken for the Pd–5.3 at % In–0.5 at % Ru alloy foil, which was subjected to electrolytic saturation with hydrogen and subsequent prolonged relaxation at room temperature and atmospheric pressure, have been analyzed. The degree of texture of the sample has been found to decrease substantially, and first-class defects in the alloy matrix dominate.
Ключевые слова
Об авторах
O. Akimova
Physical Department
Автор, ответственный за переписку.
Email: akimova@physics.msu.ru
Россия, Leninskie Gory 1, build. 2, Moscow, 119991
V. Avdyukhina
Physical Department
Email: akimova@physics.msu.ru
Россия, Leninskie Gory 1, build. 2, Moscow, 119991
I. Shchetinin
National University of Science and Technology MISIS
Email: akimova@physics.msu.ru
Россия, Leninskii pr. 4, Moscow, 119049
Дополнительные файлы