Changes in the Defect Structure of the Pd–5.3 at % In–0.5 at % Ru Alloy Subjected to Electrolytic Hydrogenation and Prolonged Relaxation
- Autores: Akimova O.V.1, Avdyukhina V.M.1, Shchetinin I.V.2
-
Afiliações:
- Physical Department
- National University of Science and Technology MISIS
- Edição: Volume 117, Nº 3 (2016)
- Páginas: 275-278
- Seção: Structure, Phase Transformations, and Diffusion
- URL: https://journals.rcsi.science/0031-918X/article/view/166666
- DOI: https://doi.org/10.1134/S0031918X16030017
- ID: 166666
Citar
Resumo
Variations in the reduced integral intensities of diffraction maxima in X-ray diffraction patterns taken for the Pd–5.3 at % In–0.5 at % Ru alloy foil, which was subjected to electrolytic saturation with hydrogen and subsequent prolonged relaxation at room temperature and atmospheric pressure, have been analyzed. The degree of texture of the sample has been found to decrease substantially, and first-class defects in the alloy matrix dominate.
Palavras-chave
Sobre autores
O. Akimova
Physical Department
Autor responsável pela correspondência
Email: akimova@physics.msu.ru
Rússia, Leninskie Gory 1, build. 2, Moscow, 119991
V. Avdyukhina
Physical Department
Email: akimova@physics.msu.ru
Rússia, Leninskie Gory 1, build. 2, Moscow, 119991
I. Shchetinin
National University of Science and Technology MISIS
Email: akimova@physics.msu.ru
Rússia, Leninskii pr. 4, Moscow, 119049
Arquivos suplementares