Evolution of the fine structure of Pd–5.3 at % Ιn–0.5 at % Ru solid solution after hydrogenation
- 作者: Akimova O.V.1, Shchetinin I.V.2
-
隶属关系:
- Physical Department
- National University of Science and Technology MISiS
- 期: 卷 117, 编号 11 (2016)
- 页面: 1119-1122
- 栏目: Structure, Phase Transformations, and Diffusion
- URL: https://journals.rcsi.science/0031-918X/article/view/166414
- DOI: https://doi.org/10.1134/S0031918X16110028
- ID: 166414
如何引用文章
详细
Fine-structure parameters, such as the effective coherent domain size Dhkl and microstrain εhkl, of Ρd–5.3 at % Ιn–0.5 at % Ru alloy foil, which was subjected to electrolytic hydrogenation and subsequent prolonged (for 55000 h) relaxation, have been determined using X-ray diffraction data. The hydrogenation and subsequent relaxation of the alloy have been found to result in the refinement of coherent domains CD(hkl) and increase in the microstrains εhkl.
作者简介
O. Akimova
Physical Department
编辑信件的主要联系方式.
Email: akimova@physics.msu.ru
俄罗斯联邦, Leninskie Gory 1, build. 2, Moscow, 119991
I. Shchetinin
National University of Science and Technology MISiS
Email: akimova@physics.msu.ru
俄罗斯联邦, Leninskii pr. 4, Moscow, 119049
补充文件