Evolution of the fine structure of Pd–5.3 at % Ιn–0.5 at % Ru solid solution after hydrogenation


Цитировать

Полный текст

Открытый доступ Открытый доступ
Доступ закрыт Доступ предоставлен
Доступ закрыт Только для подписчиков

Аннотация

Fine-structure parameters, such as the effective coherent domain size Dhkl and microstrain εhkl, of Ρd–5.3 at % Ιn–0.5 at % Ru alloy foil, which was subjected to electrolytic hydrogenation and subsequent prolonged (for 55000 h) relaxation, have been determined using X-ray diffraction data. The hydrogenation and subsequent relaxation of the alloy have been found to result in the refinement of coherent domains CD(hkl) and increase in the microstrains εhkl.

Об авторах

O. Akimova

Physical Department

Автор, ответственный за переписку.
Email: akimova@physics.msu.ru
Россия, Leninskie Gory 1, build. 2, Moscow, 119991

I. Shchetinin

National University of Science and Technology MISiS

Email: akimova@physics.msu.ru
Россия, Leninskii pr. 4, Moscow, 119049

Дополнительные файлы

Доп. файлы
Действие
1. JATS XML

© Pleiades Publishing, Ltd., 2016

Согласие на обработку персональных данных

 

Используя сайт https://journals.rcsi.science, я (далее – «Пользователь» или «Субъект персональных данных») даю согласие на обработку персональных данных на этом сайте (текст Согласия) и на обработку персональных данных с помощью сервиса «Яндекс.Метрика» (текст Согласия).