Synthesis and Physicochemical and Electrorheological Properties of Modified Nanodisperse Titanium Dioxide


Дәйексөз келтіру

Толық мәтін

Ашық рұқсат Ашық рұқсат
Рұқсат жабық Рұқсат берілді
Рұқсат жабық Тек жазылушылар үшін

Аннотация

Nanodisperse modified titanium dioxide ranging in specific surface from 70 to 130 m2/g has been prepared by a sol–gel process using Al(NO3)3 and H3PO4 as modifying components and dodecylamine and ammonium carbonate as structuring components. Microwave drying of an intermediate product and pulverization in a planetary mill have been shown for the first time to be effective in reducing the bulk density of the material and improving its electrorheological activity. The effect of filler concentration (10–40 wt %) on the shear load and leakage current density of electrorheological dispersions has been examined.

Авторлар туралы

A. Murashkevich

Belarussian State Technological University

Хат алмасуға жауапты Автор.
Email: man@belstu.by
Белоруссия, vul. Sverdlova 13a, Minsk, 220006

K. Chechura

Belarussian State Technological University

Email: man@belstu.by
Белоруссия, vul. Sverdlova 13a, Minsk, 220006

M. Novitskaya

Belarussian State Technological University

Email: man@belstu.by
Белоруссия, vul. Sverdlova 13a, Minsk, 220006

O. Alisienok

Belarussian State Technological University

Email: man@belstu.by
Белоруссия, vul. Sverdlova 13a, Minsk, 220006

E. Korobko

Lykov Institute of Heat and Mass Exchange, Belarussian Academy of Sciences

Email: man@belstu.by
Белоруссия, vul. Browki 15, Minsk, 220072

Z. Novikova

Lykov Institute of Heat and Mass Exchange, Belarussian Academy of Sciences

Email: man@belstu.by
Белоруссия, vul. Browki 15, Minsk, 220072

Қосымша файлдар

Қосымша файлдар
Әрекет
1. JATS XML

© Pleiades Publishing, Inc., 2018