Preparation of High-Purity Aluminum Oxide via Mechanochemical Oxidation of Aluminum in a 0.1 M KOH Solution, Followed by Chemical and Heat Treatments


Citar

Texto integral

Acesso aberto Acesso aberto
Acesso é fechado Acesso está concedido
Acesso é fechado Somente assinantes

Resumo

We have examined the feasibility of preparing high-purity aluminum oxide by oxidizing granulated aluminum in a 0.1 M potassium hydroxide solution, followed by heat and acid treatments of the oxidation products. The aluminum oxidation product, consisting of two phases of Al(OH)3 (bayerite and gibbsite), was first heat-treated at temperatures of 300, 600, 900, and 1200°C; then treated with hydrochloric acid; and calcined at a temperature of 1450°C. It has been shown that raising the preheat treatment temperature increases the total concentration of impurities, including Fe impurities, but reduces the concentration of alkali metals (K, Na, and Li). Using 99.7%-pure aluminum, we have prepared aluminum oxide with a purity at a level of 99.886%. Using 99.98%-pure aluminum, we have obtained aluminum oxide with a purity at a level of 99.993%.

Sobre autores

G. Ambaryan

Joint Institute for High Temperatures, Russian Academy of Sciences

Autor responsável pela correspondência
Email: ambaryan1991@gmail.com
Rússia, Izhorskaya ul. 13/2, Moscow, 125412

M. Vlaskin

Joint Institute for High Temperatures, Russian Academy of Sciences

Email: ambaryan1991@gmail.com
Rússia, Izhorskaya ul. 13/2, Moscow, 125412

A. Zhuk

Joint Institute for High Temperatures, Russian Academy of Sciences

Email: ambaryan1991@gmail.com
Rússia, Izhorskaya ul. 13/2, Moscow, 125412

E. Shkol’nikov

Joint Institute for High Temperatures, Russian Academy of Sciences

Email: ambaryan1991@gmail.com
Rússia, Izhorskaya ul. 13/2, Moscow, 125412

Arquivos suplementares

Arquivos suplementares
Ação
1. JATS XML

Declaração de direitos autorais © Pleiades Publishing, Inc., 2019